bp15da4
Standoff Arc voltage
Lag lines
Figure 4-4. Cut quality
Positive (+) cut angle A
Bottom dimension “B is greater than
dimension “A”
B
Negative (-) cut angle A
Bottom dimension “B is less than
dimension “A”
B
Figure 4-5. Cut angle
7.5 Dross formation
Cutting speed, gas selection and variations in metal composition contribute to dross
formation. The correct cutting standoff also has an influence on dross formation. If
the arc voltage is set too high, the cut angle becomes positive. In addition, dross
forms on the bottom edge of the part. This dross can be very tenacious and require
chipping and grinding for removal. Setting the cutting voltage too low results in
undercutting the parts or negative cut angle. Dross formation occurs but in most
cases it is easily removed.